Alloy 188
A Cobalt-based alloy, Alloy 188 has excellent high temperature strength.
SPECIFICATIONS
UNS Number: UNS R30188
W.Nr.Number: 2.4683
Standards: AMS 5608, AMS 5801, AMS 5772
| PRODUCT FORM |
SIZE RANGE FROM |
SIZE RANGE TO |
| Alloy 188 round bar |
10 mm |
168 mm |
| Alloy 188 sheet & plate |
0.38 mm |
50.8 mm |
| Alloy 188 welding wire |
0.635 mm |
2.36 mm |
Cobalt Alloy 188 Chemical properties
| % |
Cr |
Ni |
Co |
W |
La |
B |
C |
Fe |
Mn |
Si |
P |
S |
| Min |
20 |
20 |
- |
13 |
0.02 |
- |
0.05 |
- |
- |
0.2 |
- |
- |
| Max |
24 |
24 |
Balance |
16 |
0.12 |
0.015 |
0.015 |
3 |
1.25 |
0.5 |
0.02 |
0.015 |
Cobalt Alloy 188 Mechanical & Physical Properties
| |
21°C |
427°C |
538°C |
649°C |
760°C |
871°C |
982°C |
1093°C |
| Ultimate Tensile Strength /MPa |
944.6 |
- |
- |
710.2 |
620.5 |
413.7 |
241.3 |
131 |
| 0.2% Yield Strength /MPa |
462 |
- |
- |
275.8 |
268.9 |
248.2 |
131 |
62.1 |
| Elongation % |
53 |
- |
- |
59 |
63 |
64 |
59 |
- |
| Coefficient of Thermal Expansion µm/m⁰C |
- |
14 |
14.8 |
15.5 |
16.2 |
16.9 |
17.8 |
- |
| Thermal Conductivity /kcal/(hr.m.°C) |
- |
15.5 |
17.1 |
18.9 |
20.7 |
21.6 |
23.5 |
- |
| Modulus of Elasticity/ x105 MPa |
2.34 |
2 |
1.93 |
1.79 |
1.72 |
1.65 |
1.52 |
- |
Alloy L605/25
A cobalt-chromium-nickel-tungsten superalloy, L605/25 is one of the strongest cobalt alloys.
SPECIFICATIONS
UNS Number: UNS R30605
W.Nr.Number: 2.4964
Standards: AMS 5537, 5796
| PRODUCT FORM |
SIZE RANGE FROM |
SIZE RANGE TO |
| Alloy L605/25 round bar |
5.2 mm |
168.3 mm |
| Alloy L605/25 sheet & plate |
0.25 mm |
38.1 mm |
| Alloy L605/25 welding wire |
0.8 mm |
2.36 mm |
Cobalt Alloy L605/25 Chemical properties
| % |
Cr |
Ni |
Co |
W |
C |
Fe |
Mn |
Si |
P |
S |
| Min |
19 |
9 |
- |
14 |
0.05 |
- |
1 |
- |
- |
|
| Max |
21 |
11 |
Balance |
16 |
0.15 |
3 |
2 |
0.4 |
0.04 |
0.03 |
| Mechanical & Physical Properties |
21°C |
427°C |
538°C |
649°C |
760°C |
816°C |
871°C |
927°C |
982°C |
| Coefficient of Thermal Expansion µm/m⁰C |
- |
14 |
14.4 |
14.8 |
15.5 |
- |
16.4 |
- |
16.9 |
| Thermal Conductivity /kcal/(hr.m.°C) |
- |
14.9 |
16.7 |
18.6 |
20.4 |
- |
22.6 |
- |
24.8 |
| Modulus of Elasticity/ x105 MPa |
2.28 |
1.93 |
1.86 |
1.79 |
1.65 |
- |
1.59 |
- |
1.45 |
| Ultimate Tensile Strength /Mpa |
1006.6 |
- |
- |
744.6 |
641.2 |
- |
413.7 |
- |
234.4 |
| 0.2% Yield Strength /MPa |
475.7 |
- |
- |
331 |
282.7 |
- |
248.2 |
- |
124.1 |
| Elongation/ % |
51 |
- |
- |
60 |
42 |
- |
45 |
- |
32 |
| 100 hr Rupture Strength/ Mpa |
- |
- |
- |
475.7 |
248.2 |
172.4 |
124.1 |
82.7 |
48.3 |
| 1000 hr Rupture Strength/ Mpa |
- |
- |
- |
393 |
179.3 |
124.1 |
82.7 |
48.3 |
27.6 |
Cobalt-based alloys
| Product |
UNS Number |
| ATI 35N™ |
R30035 |
| ATI 188™ |
R30188 |
| ATI L-605™ |
R30605 |
| TJA-1537® |
R31537 & R31538 |